Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF20 - PA6 Nylon 6, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 20% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF30 - PA6 Nylon 6, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF40 - PA6 Nylon 6, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-GP2-[color]-H General Purpose Nylon 66, Nucleated, Heat Stabilized General Purpose Nylon 66, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM2-[color]H Nylon, Superior Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM2-LM Nylon, Preliminary Data Sheet, Low Flexural Modulus, High Impact (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-MD-[color]-H Nylon 66, 2% MoS2 Nylon 66, 2% Molybdenum Disulfide for Lubrication and Wear, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-MD02 Nylon, 2% Molybdenum disulfide for lubrication and wear (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-MD1 Nylon 66, 1% MoS2 Nylon 66, 1% Molybdenum Disulfide for Lubrication and WearProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon.. |
|||
Front Barrel Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PlastiComp Complet® LCF30 - PA6 Nylon 6, 30% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 30% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM1 Nylon 66, Medium Impact Modified Nylon 66, Medium Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are te.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-IM1-[color]-H Nylon 66, Medium Impact Modified, Heat Stabilized Nylon 66, Medium Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Ny.. |
|||
Front Barrel Temperature | 277 - 288 °C | 530 - 550 °F | |
Polymer Resources NY66-MD02-[color]-H Nylon, 2% Molybdenum disulfide for lubrication and wear, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 246 - 288 °C | 475 - 550 °F | |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 246 - 288 °C | 475 - 550 °F | |
Star Plastics PC/ABSQX7002 Molding Grade PC/ABS High Flow Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 271 - 288 °C | 520 - 550 °F | |
Samyang Trirex® PC-3022IR 15 MFI Clear Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |