Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 350 - 421 °C | 662 - 790 °F | Average value: 387 °C Grade Count:15 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7033 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8032/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8084/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8086/YL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8088/RD Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8124 Polyether imide, lubricant modified Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1500-0871 Polysulfone, with glass spheres Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1500-8299 Polysulfone, with PTFE, lubricant modified Applications: Isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precision parts, high continuous use temperature.Control disks, ca.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7743 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8133 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8154/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika L-1003PA Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 370 °C | 662 - 698 °F | |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Nozzle Temperature | 350 - 400 °C | 662 - 752 °F | |
Lehmann & Voss LUVOCOM® 1106-7940/GY Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |