Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Mold Temperature | 77.0 - 116 °C | 171 - 241 °F | |
Albis Plastics PC/PET 748/718 GF 20 HZ 20% Glass Fiber
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-FR1A-D-[color]-3 Polycarbonate, Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Mold Temperature | 65.6 - 116 °C | 150 - 240 °F | Average value: 85.7 °C Grade Count:8 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Mold Temperature | 65.6 - 116 °C | 150 - 241 °F | Average value: 80.3 °C Grade Count:7 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled 20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 82.0 - 116 °C | 180 - 241 °F | |
Styron EMERGEâ„¢ 4702-8 Polycarbonate EMERGEâ„¢ PC 4702-8 advanced resin is formulated with 20% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat resi.. |
|||
Mold Temperature | 82.0 - 116 °C | 180 - 241 °F | |
Styron EMERGEâ„¢ 4731-13 Polycarbonate EMERGEâ„¢ PC 4731-13 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability .. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |