Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, PTFE Filled
Manufacturer Polymer Resources, LTD
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 7.0 - 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.0 - 12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.2 MPa
8000 psi
ASTM D638
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm

@Temperature 22.8 °C
3.00 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Gardner Impact 36.2 J
26.7 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
278 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
267 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 288 - 310 °C
550 - 590 °F
Middle Barrel Temperature 299 - 321 °C
570 - 610 °F
Front Barrel Temperature 310 - 332 °C
590 - 630 °F
Melt Temperature 316 - 343 °C
600 - 650 °F
Mold Temperature 82.2 - 116 °C
180 - 240 °F
Drying Temperature 118 - 124 °C
245 - 255 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Descriptive Properties Value Comments
Vent 0.0005