Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Rear Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT2202-732UV Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Box top railTail gate linerExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Exterior componentsBodyside moldingsStep padsLicense plate bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-659UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-559UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM WPP 646H) Charcoal Metallic Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products GC10P100-00 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products GC10P100-01 10% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Air ducts - distributionFuel filler pocketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products GC10P200-01 10% Glass Fiber Reinforced Polypropylene Copolymer, Non-UV Stabilized, Chemically Coupled, Black Applications: HousingsStorage binsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-434 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9648 Medium Dark Neutral Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-186 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-231 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 173B Navy Blue Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M12P100-01 12% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsFiller panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-00 14% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-288UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167A Ebony Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/40/E High performance polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |