Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
Multibase Multi-Pro® 3014 XUGW Polypropylene Mineral Filled.Features:Gloss, HighUV Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:FurnitureLawn and Garden EquipmentInformation provided by Multibase |
|||
Rear Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Multibase Multi-Pro® 3018 TU Polypropylene Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
Multibase Multi-Pro® 3018 XUG Polypropylene Mineral Filled, 30% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureInformation provided by Multibase |
|||
Rear Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Multibase Multi-Pro® 4009 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Lawn and Garden EquipmentTable ProductsFurnitureInformation provided by Multibase |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4700-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-74UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-00UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Natural Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products G13P100-01 13% Glass Fiber Reinforced Polypropylene, Black Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products GC15P200-00 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-01 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-182 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 7701 Graphite Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP520-01 12% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Interior trimCenter consolesGlove box binsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP521-229 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Interior trimIP structural componentsScuff/kick platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP522-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M12P250-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Filler panelsHVAC ductsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T10P250-00 10% Talc Reinforced Polypropylene Copolymer, Natural Applications: Fan shroudsCenter consolesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products T12P600-01BG 12% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: Flipper panelClose out panelSeat backsLoad floorInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Fiberfil® J-69/10/E/UV High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Rear Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |