Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 - 180 °C | 302 - 356 °F | Injection |
Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Extrusion |
Stellarchem 8075 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Extrusion |
Stellarchem GP-785A TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | Injection Molding |
Stellarchem MP-930HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Rear Barrel Temperature | 150 - 160 °C | 302 - 320 °F | Extrusion |
Stellarchem SV-B40D TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Rear Barrel Temperature | 150 - 160 °C | 302 - 320 °F | Extrusion |
Stellarchem SV-B70E TPV Compound This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on .. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Cast film |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Cast film |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Cast film |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Blown film |
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 2112 AC Ethylene and 12% Ethyl Acrylate Copolymer Elvaloy® 2112 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for tubing is various applications. The.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 2615 AC Ethylene and 15% Ethyl Acrylate Copolymer Because of its high flexibility and high filler loading capacity, Elvaloy® 2615 AC is particularly suited for injection molded parts in the automotive and furniture industries. It also offers exce.. |
|||
Rear Barrel Temperature | 150 - 170 °C | 302 - 338 °F | |
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | For high temperature coextrusions. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | Extrusion lamination and extrusion coating |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | For high temperature coextrusions. |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |
|||
Rear Barrel Temperature | 150 °C | 302 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |