Material Notes:
Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylene (PP) resins.Applications:Bynel® Series 5000 resins adhere to a variety of materials. They are most often used to adhere to PP, EVOH, and polyamide. These resins are designed for applications in which EVOH or polyamide is melt coextruded with PP or PP copolymers.Bynel® 50E662 can be used in coextrusion processes including blown film, extrusion blow molding, melt and solid phase thermoforming, and cast film or sheet.Physical properties of Bynel® Series 5000 resins are typical of polypropylene resins with similar density and melt index values. Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 105 °C
221 °F
Freezing Point, DSC; ASTM D3418
150 °C
302 °F
DSC; ASTM D3418
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 150 °C
302 °F
For high temperature coextrusions.
150 °C
302 °F
For coextrusion with EVA or EVOH.
Middle Barrel Temperature 220 °C
428 °F
For coextrusion with EVA or EVOH.
235 °C
455 °F
For high temperature coextrusions.
Front Barrel Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
250 °C
482 °F
For high temperature coextrusions.
Adapter Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
250 °C
482 °F
For high temperature coextrusions.
Die Temperature 235 °C
455 °F
For coextrusion with EVA or EVOH.
250 °C
482 °F
For high temperature coextrusions.
Users viewing this material also viewed the following: