Processing Properties Metric English Comments
Drying Temperature 100 - 115 °C

@Time 10800 - 21600 sec
212 - 239 °F

@Time 3.00 - 6.00 hour
Pre-dry
Kingfa JH830 Flame Retardant PC
Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov..
Drying Temperature 100 - 115 °C

@Time 10800 - 14400 sec
212 - 239 °F

@Time 3.00 - 4.00 hour
Pre-dry
Kingfa PC-S609 Toughened PC
Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl..
Drying Temperature 105 - 115 °C

@Time 10800 - 14400 sec
221 - 239 °F

@Time 3.00 - 4.00 hour
Pre-dry
Kingfa PC-S809 Modified PC
Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl..
Drying Temperature 105 - 115 °C
221 - 239 °F
Injection Molding
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant
Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical