Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 93.0 °C @Time 7200 sec |
199 °F @Time 2.00 hour |
|
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 30% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Drying Temperature | 93.0 °C @Time 7200 sec |
199 °F @Time 2.00 hour |
|
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Drying Temperature | 93.0 °C @Time 7200 sec |
199 °F @Time 2.00 hour |
|
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Drying Temperature | 93.0 °C @Time 7200 sec |
199 °F @Time 2.00 hour |
|
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 60% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Drying Temperature | 93.0 °C | 199 °F | |
PolyOne Lubri-Tech™ PS-30GF/ 02S PBT Polyester - 30% Glass Fiber - 2% Silicone
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 °C | 199 °F | |
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-000/40T Nylon 6/12 - 40% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-10GF/15TF Nylon 6/12 - 10% Glass Fiber - 15% PTFE Flock
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 - 107 °C | 199 - 225 °F | |
PolyOne Lubri-Tech™ NL-15KV/05M Nylon 6/12 - 15% Kevlar Fiber - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | <= 93.0 °C | <= 199 °F | |
Lord Adhesives Chemlok® 5150 Adhesive LORD Chemlok® 5150 adhesive is a solvent-based adhesive used to bond uncured fluoroelastomers to metal. It can also be used to bond fluoroelastomers with an incorporated cure system to mechanical.. |
|||
Drying Temperature | 93.0 °C | 199 °F | |
PolyOne Lubri-Tech™ MP-20GF/15T Modified PPO - 20% Glass Fiber - 15% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 °C | 199 °F | |
PolyOne Stat-Tech™ MP-25NCF/000 Modified PPO - 25% Nickel Coated Graphite Fiber
(discontinued **) Data provided by PolyOne. |
|||
Drying Temperature | 93.0 °C | 199 °F | |
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced
(discontinued **) Data provided by PolyOne. |