Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.084 g/cc
0.03916 lb/in³
ASTM D792
Water Absorption 0.35 %
0.35 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm

@Thickness 3.17 mm
0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 66.0 MPa
9570 psi
ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
ASTM D638
Tensile Modulus 4.50 GPa
653 ksi
ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 4.50 GPa
653 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm

@Thickness 6.35 mm
2.00 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 238 - 271 °C
460 - 520 °F
Stock
Mold Temperature 93.0 °C
199 °F
Drying Temperature 93.0 °C
199 °F