Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.342 g/cc
0.04848 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.010 - 0.020 cm/cm

@Thickness 3.17 mm
0.010 - 0.020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 2.0 - 5.0 %
2.0 - 5.0 %
ASTM D638
Tensile Modulus 2.10 GPa
305 ksi
ASTM D638
Flexural Yield Strength 76.0 MPa
11000 psi
ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 0.430 - 0.690 J/cm

@Thickness 6.35 mm
0.806 - 1.29 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Stock
Mold Temperature 93.0 - 107 °C
199 - 225 °F
Drying Temperature 93.0 - 107 °C
199 - 225 °F