Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoro.. |
|||
Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Back Pressure | 0.517 - 0.862 MPa | 75.0 - 125 psi | |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Back Pressure | 0.000 - 0.862 MPa | 0.000 - 125 psi | |
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE) Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-1069A Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-1069E2 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-1373G Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-1674C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2023 Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2028A UMB Thermoplastic Elastomer Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2598A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2640S Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2678C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7010-40D-NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7010-64NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7010-73NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7010-80NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7100-87 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7200-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Automotive Specifications: Chrysler MS-AK91; FORD WSS-M2D510-A7; .. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2533A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7010-55NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7100-40D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7100-64 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-7100-80 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |