Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Melt Flow 12.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 15
15
1 second; ASTM D2240
Tensile Strength at Break 2.07 MPa
300 psi
ASTM D412
Elongation at Break 480 %
480 %
ASTM D412
Processing Properties Metric English Comments
Rear Barrel Temperature 173 - 213 °C
344 - 416 °F
Middle Barrel Temperature 179 - 219 °C
354 - 426 °F
Front Barrel Temperature 184 - 224 °C
364 - 436 °F
Nozzle Temperature 190 - 230 °C
374 - 446 °F
Zone 1 166 - 204 °C
330 - 400 °F
Zone 2 171 - 210 °C
340 - 410 °F
Zone 3 177 - 216 °C
350 - 420 °F
Zone 5 182 - 221 °C
360 - 430 °F
Die Temperature 190 - 227 °C
374 - 440 °F
Melt Temperature 190 - 230 °C
374 - 446 °F
Processing Temperature
Mold Temperature 35.0 - 60.0 °C
95.0 - 140 °F
Injection Pressure 1.38 - 6.89 MPa
200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa
25.0 - 125 psi
Cushion 0.381 - 2.54 cm
0.150 - 1.00 in
Screw Speed 50 - 120 rpm
50 - 120 rpm
Descriptive Properties Value Comments
Appearance Opaque