Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Back Pressure = 40.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-B30 PTFE
Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 40.0 - 50.0 MPa
5800 - 7250 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-G15 PTFE
Tarflen SM1 reinforced with 15% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-G20 PTFE
Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-K25 PTFE
Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-K22G3 PTFE
Tarflen SM1 reinforced with 22% coke and 3% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.