Azoty Tarnow™ TARFLEN SM-K25 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Azoty Tarnow™ (Zaklady Azotowe)
Trade Name TARFLEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azoty Tarnow™ TARFLEN SM-K25 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.11 g/cc
0.0762 lb/in³
ISO 1183
Filler Content 25 %
25 %
Coke
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Ball Indentation Hardness 50.0 MPa
7250 psi
ISO 2039-1
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527
Elongation at Break 120 %
120 %
ISO 527
Izod Impact, Notched 1.20 J/cm
2.25 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 64000 ohm-cm
64000 ohm-cm
IEC 60093
Surface Resistance 64000 ohm
64000 ohm
IEC 60093
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure