Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except.. |
|||
Screw Speed | 80 - 120 rpm | 80 - 120 rpm | |
PolyOne Versaflex™ OM 6275-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6275-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. New Prod.. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1033STHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N2000STHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1013L Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 40 - 120 rpm | 40 - 120 rpm | |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP PBT 1100-211X Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP PBT 1100-630S Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP ABS/PBT 7320H-104 20% Glass Fiber Filled Product Description: A 20% glass fiber reinforced injection molding grade. Characteristics:Low warp age and excellent dimensionally stable Excellent electrical property Excellent mechanic and chemi.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 2000-104D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax PBT 3020-104 15% Glass Fiber Filled Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2420B Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2598D Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-2598E Thermoplastic Vulcanizate Alloy Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66 Description: Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® FRGF25-66-N Flame Retardant Nylon 66, Lubricated, 25% Glass Fiber Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous.. |
|||
Screw Speed | 30 - 120 rpm | 30 - 120 rpm | |
Wellman Wellamid® GB1430-N 33% Glass Bubble Filled, Low Density Nylon 66 Description: Glass Bubble Filled, Low Density Nylon 66Information provided by Wellman. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Screw Speed | 50 - 120 rpm | 50 - 120 rpm | |
Teknor Apex Uniprene® UN-7100-73 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP PBT 3010-104 10% Glass Fiber Filled Product Description: PBT glass fiber 10% reinforced injection molding grade.Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent.. |
|||
Screw Speed | 60 - 120 rpm | 60 - 120 rpm | to be chosen in such a way that plasticizing time is just within cooling time |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |