Polymer Property : Cure Time = 0.00972 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 0.583 - 1.00 min
0.00972 - 0.0167 hour
On Steel (Fixture)
ND Industries High Temperature SuperGlue 311
Very high viscosity with thermal cycling resistance
Cure Time 0.583 - 0.833 min
0.00972 - 0.0139 hour
Aluminum, handling time
Permabond 735 Cyanoacrylate, toughened
PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Cure Time 0.583 - 3.00 min
0.00972 - 0.0500 hour
Average value: 1.63 min Grade Count:5
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Cure Time 0.583 - 1.58 min
0.00972 - 0.0264 hour
Gelation time
Mitsui MILEXâ„¢ RN-2830MR Acrylic Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Cure Time 0.583 - 1.25 min
0.00972 - 0.0208 hour
Tack Free Time
ACC EP IS EPI Engineered Polymers Integral Skin Flexible Foam
EP-IS is integral skin flexible foam, “Powered by Reactamine ® Technology”, designed to give excellent surface skin. EP-IS contains cyclopentane as its blowing agent, which conforms to EPA standa..