Processing Properties Metric English Comments
Cure Time 2.00 - 3.00 min
0.0333 - 0.0500 hour
Aluminum, handling time
Permabond 731 Cyanoacrylate, toughened
PERMABOND® 731 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o..
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
handling time
Permabond TA436 Toughened Acrylic Adhesive
PERMABOND TA436 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. Permabond TA436 is a no-mix system which obtains handling strength..
Cure Time 0.583 - 3.00 min
0.00972 - 0.0500 hour
Average value: 1.63 min Grade Count:5
Overview of materials for Phenolic/Rubber; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp..
Cure Time 1.00 - 3.00 min

@Temperature 204 - 260 °C
0.0167 - 0.0500 hour

@Temperature 399 - 500 °F
Lord Adhesives Flocklok® 550P Flock Adhesive
LORD Flocklok® 550P adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of uncured and semi-cured elastomers including EPDM, NR, CR and SBR. Flocked sub..
Cure Time 2.00 - 3.00 min
0.0333 - 0.0500 hour
Working time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Ultra White
Information provided by ITW Devcon
Cure Time 1.00 - 3.00 min

@Temperature 140 - 160 °C
0.0167 - 0.0500 hour

@Temperature 284 - 320 °F
Lucite International Colacryl ® TS1631 Acrylic Solution Resin
Acrylic copolymer with reactive groupsA highly flexible resin with good handle. It exhibits good adhesion, resistance to ageing and light stability.Suggested Use: Coating and lamination of nylon and..
Cure Time 1.17 - 3.00 min
0.0194 - 0.0500 hour
Gelation time
Mitsui MILEXâ„¢ RN-2830MB Acrylic Rubber Modified Phenolic Resin
The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad..
Cure Time 2.50 - 3.00 min

@Temperature 150 °C
0.0417 - 0.0500 hour

@Temperature 302 °F
Loctite® 3607 Pin Transfer
Surface Mount AdhesivesLoctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application te..
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-30 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-31 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-32 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-33 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-34 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-35 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-36 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-37 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 1.00 - 3.00 min
0.0167 - 0.0500 hour
Setting Time
Chosun Refractories HSM-38 Heat-Setting Mortar
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Cure Time 0.750 - 3.00 min
0.0125 - 0.0500 hour
Time to Handling Strength