Polymer Property : Cure Time = 0.333 hour Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 10.0 - 20.0 min
0.167 - 0.333 hour
On steel (Fixture)
ND Industries 530 Shaft & Bearing Retainer Retaining Compound
General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec ..
Cure Time 5.00 - 20.0 min
0.0833 - 0.333 hour
for compression molded lab sheets
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
Cure Time 15.0 - 20.0 min
0.250 - 0.333 hour
Working time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive II, Straw, Black
Information provided by ITW Devcon
Cure Time 15.0 - 20.0 min
0.250 - 0.333 hour
Fixture time
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive SD, Off-White
Information provided by ITW Devcon
Cure Time 15.0 - 20.0 min
0.250 - 0.333 hour
Tack-free time
Master Bond MasterSil 705S Silver Filled, Non-Corrosive Silicone
Description: Master Bond MasterSil 705S is an easy-to-use, one component, non-corrosive, electrically conductive, silver filled, silicone for bonding and sealing. The material is a gray colored past..
Cure Time 15.0 - 20.0 min
0.250 - 0.333 hour
Tack-free time
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec
Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL..
Cure Time 5.00 - 20.0 min
0.0833 - 0.333 hour
for compression molded lab sheets
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
Cure Time 15.0 - 20.0 min
0.250 - 0.333 hour
Time to Handling Strength
3M Scotch-Weld™ DP605NS Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..
Cure Time 10.0 - 20.0 min
0.167 - 0.333 hour
Time to Handling Strength
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Cure Time 10.0 - 20.0 min
0.167 - 0.333 hour
Time to Handling Strength
3M Scotch-Weld™ DP810NS Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Cure Time 10.0 - 20.0 min
0.167 - 0.333 hour
Time to Handling Strength
3M Scotch-Weld™ DP100 FR Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP100 FR is a two-part flame retardant (self-extinguishing) version of Scotch-Weld DP100. It meets the UL94 V-O Burn Test requirements and has a work life of 4-8 mi..
Cure Time 15.0 - 20.0 min

@Temperature 24.0 °C
0.250 - 0.333 hour

@Temperature 75.2 °F
BCC Products BC 4570 Polyester Hi Heat Filler
BC 4570 is a multi-purpose paste designed for making quick repairs to a variety of substrates where service temperature exceeds 200º F (93º C). It is easy to mix and apply, cures in 15-20 minutes ..
Cure Time 10.0 - 20.0 min
0.167 - 0.333 hour
Time to Handling Strength
3M Scotch-Weld™ DP810 Tan Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
Cure Time 5.00 - 20.0 min
0.0833 - 0.333 hour
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System
Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru..