Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | On steel (Fixture) |
ND Industries 541 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft |
|||
Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | On steel (Fixture) |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | working strength |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Cure Time | 30.0 - 40.0 min @Temperature 25.0 °C |
0.500 - 0.667 hour @Temperature 77.0 °F |
Handling strength |
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Cure Time | 30.0 - 40.0 min @Temperature 25.0 °C |
0.500 - 0.667 hour @Temperature 77.0 °F |
Handling strength |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Cure Time | 30.0 - 40.0 min | 0.500 - 0.667 hour | Working time |
ITW Devcon Safety Clear Coatâ„¢ Epoxy, Water Clear Information provided by ITW Devcon |
|||
Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | Setting Time |
Chosun Refractories APC-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Cure Time | 20.0 - 40.0 min | 0.333 - 0.667 hour | Setting Time |
Chosun Refractories APC-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |