Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Plastcom SLOVALEN PH 51 T 40 Polypropylene Homopolymer, 40% Micronized Talc
FeaturesModified homopolymer PP for injection moulding with the content of 40% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden..
Melt Temperature 200 - 250 °C
392 - 482 °F
Plastcom SLOVALEN PH 51 T 60 PP, 60% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 60% microground, floated, chemically modified talc. General application in all industry. Delivered in natural mode and in t..
Melt Temperature 200 - 250 °C
392 - 482 °F
Plastcom SLOVALEN PH 66 GF 20 FRO 4 PP, 20% glass fibre, flame retardant
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass fibre, with decreased flammability. Used in the electrical industry - teroderately increased toughness an..
Melt Temperature 200 - 250 °C
392 - 482 °F
Premix Thermoplastics PRE-ELEC® PE 1292
PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129..
Melt Temperature 200 - 250 °C
392 - 482 °F
Premix Thermoplastics PRE-ELEC® PP 1373
PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Melt Temperature 200 - 250 °C
392 - 482 °F
Premix Thermoplastics PRE-ELEC® PP 1375
PRE-ELEC PP 1375 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE..
Melt Temperature 230 - 250 °C
446 - 482 °F
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Melt Temperature 230 - 250 °C
446 - 482 °F
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified
Information provided by Polykemi AB
Melt Temperature 230 - 250 °C
446 - 482 °F
Polykemi AB POLYfill PP CQX30030 RTX Polypropylene, Mineral Reinforced, Scratch Resistant
Information provided by Polykemi AB
Melt Temperature 200 - 250 °C
392 - 482 °F
Plastcom SLOVALEN PH 49 GF 30 003/3M Polypropylene reinforced with glass fiber, heat stabilized
Modified homopolymer PP for injection molding, reinforced with 30% glass fiber, heat stabilized. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Melt Temperature 230 - 250 °C
446 - 482 °F
Start Point: 240°C
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an..
Melt Temperature 220 - 250 °C
428 - 482 °F
Injection Molding
LG Chemical LUCON PS4200 ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch..
Melt Temperature 240 - 250 °C
464 - 482 °F
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Melt Temperature 240 - 250 °C
464 - 482 °F
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Melt Temperature 220 - 250 °C
428 - 482 °F
LG Chemical PI-642 ABS, Fitting, High Strength
Information Provided by LG Chem
Melt Temperature 200 - 250 °C
392 - 482 °F
Extrusion Molding
LG Chemical SH625 ABS, High Impact, High Flow
Feature: Extrusion Molding, High Impact, High FlowApplication: Ski Flat, MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical
Melt Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 200NH PC/ABS alloy, Flame Retardant
Non-halogenCharacteristics:Impact resistantDimensional stabilityProcessabilityApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang
Melt Temperature 190 - 250 °C
374 - 482 °F
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, conditioned
Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
Melt Temperature 190 - 250 °C
374 - 482 °F
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry
Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact..
Melt Temperature 220 - 250 °C
428 - 482 °F
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled
SAXALEN PPH335T20 is a 20% mineral filled Polypropylene - Homopolymer intended for injection molding with very good flow properties and higher stiffness by low warpage and good surface appearance.In..
Melt Temperature 230 - 250 °C
446 - 482 °F
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications
Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Melt Temperature 210 - 250 °C
410 - 482 °F
Borealis HJ320MO Polypropylene
HJ320MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. This grade is ..
Melt Temperature 235 - 250 °C
455 - 482 °F
DAM; Extrusion
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6  (Unverified Data**)
Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an..
Melt Temperature 210 - 250 °C
410 - 482 °F
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding
Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded
Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar.
Melt Temperature 225 - 250 °C
437 - 482 °F
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded
Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar.
Melt Temperature 230 - 250 °C
446 - 482 °F
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT
Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe..
Melt Temperature 207 - 250 °C
405 - 482 °F
Average value: 227 °C Grade Count:29
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
Melt Temperature 180 - 250 °C
356 - 482 °F
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate
Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym..
Melt Temperature 200 - 250 °C
392 - 482 °F
Injection Molding
Polimeri Europa Edistir N 1910 Polystyrene
Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear..