Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 235 - 245 °C | 455 - 473 °F | |
Polyplastic Armamid® PA 6-1FR Nylon 6, Flame Retardant Halogen and phosphor freeInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-117 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-220 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-301 Flame Retardant Polystyrene Features:UL 94 V-1 @ 2.0 & 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingElectrica.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-702 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa HR-527 Modified ABS Features:UL94 HB @ 1.5-3.2mmImpact resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 230 - 245 °C | 446 - 473 °F | Extrusion Molding |
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical LUPOS HR2207A ABS+GF20%, General Purpose, Heat Resistance Feature: Injection Molding, ABS+GF20%, General Purpose, Heat ResistanceApplication: Electric & Electronic (Housing, Components)Information provided by LG Chemical |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Melt Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-100 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mmLow smoking, low halogenExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV or aud.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-722 Flame Retardant Polystyrene Features:UL 94 V-0 @ 3.2mmHalogen free flame retardantExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElectrical appliance housing.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | Start Point: 230°C |
Kingfa FRHIPS-930 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec.. |
|||
Melt Temperature | 220 - 245 °C | 428 - 473 °F | |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | Extrusion |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Ultramid® HFX 37 PA6 (Dry) Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
Huntsman Rexell® L8404 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, and FDA compliant.Applications: Blown film extrusion: general purpose.Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by H.. |
|||
Melt Temperature | 205 - 245 °C | 401 - 473 °F | |
Huntsman Rexell® L8101 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.Applications: Sealing layer in coextr.. |