Sylvin Technologies 916V0 Black PVC for Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 916V0 Black PVC for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
Thickness 3000 microns
118 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 seconds
Tensile Strength, Ultimate 15.5 MPa
2250 psi
Elongation at Break 320 %
320 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
RTI
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Comparative Tracking Index 400 - 600 V
400 - 600 V
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
High Amp Arc Ignition, HAI 30 - 60 arcs
30 - 60 arcs
Processing Properties Metric English Comments
Melt Temperature 171 - 182 °C
340 - 360 °F