Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | Extrusion |
DuPont Performance Polymers Hytrel® HTR8730 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8730 BK320 is a high viscosity thermoplastic polyester elastomer designed for blow molding. It has excellent mechanical properties at elevated temperatures and very good resistance to mo.. |
|||
Melt Temperature | 225 - 310 °C | 437 - 590 °F | Average value: 272 °C Grade Count:13 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Melt Temperature | 225 °C | 437 °F | |
Iran Petrochemical (PCC) LL0209 SR Linear Low Density Polyethylene LL 0209 is a LLDPE copolymer with butene as comonomer which contains anti-oxidant, Slip and antiblock additives. It gives film of high slip which is easily separable. It is recommended for general .. |
|||
Melt Temperature | 225 °C | 437 °F | LCL-PR29 |
Intercontinental Polymers HoPBT 550 HoPBT Polymer Type - Clear, Polyester Pellets Applications: Engineering Resin Information provided by Intercontinental Polymers. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0209 KJ LLDPE Film Applications:Refuse sacksProduce bags, carrier bagsFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0220 AA LLDPE Film Applications:Light and medium duty filmStretch filmFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor o.. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Melt Temperature | 225 °C | 437 °F | |
SIDPEC EGYPTENE® LL 0205 AF LLDPE Film Applications:Heavy duty sacks, mulch filmsStretch film, liners, geomembraneFilm properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l... |
|||
Melt Temperature | <= 225 °C | <= 437 °F | |
Tipco Tipwood® 50 EX 50EX Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen.. |
|||
Melt Temperature | 225 - 260 °C | 437 - 500 °F | |
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HW 30K ECR-BK PP, Injection Molded Starpylen HW 30K ECR-BK is a reinforced Polypropylene with a low carbon footprint spherical filler, Injection Molding Resin (also known as HW30KECR)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF003SU PP, 15% Glass Fiber Filled, Injection Molded Starpylen MF003SU is a 15% Glass Fiber Reinforced Polypropylene Injection Molding Resin (also known as Starpylen WX 15V S34/040)Information provided by Eurostar. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | Extrusion |
DuPont Performance Polymers Hytrel® G5564 TPC-ET
(Unverified Data**) Hytrel® G5564 is a 55 nom. Shore D, heat stable, plasticiser free high viscosity resin for extrusion; low temperature impact resistance as well as excellent mechanical properties; good hydrocarbon .. |
|||
Melt Temperature | 225 °C | 437 °F | Optimum; Extrusion |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Melt Temperature | 225 - 280 °C | 437 - 536 °F | |
Beijing Ranger Chem PBT 403 G-M50 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT 403 M-G10 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT 403 M-G30 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 245 °C | 437 - 473 °F | |
Beijing Ranger Chem PBT-MFC-G0 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 °C | 437 °F | Extrusion Coating |
Braskem CN8092 EVA Molding Copolymer CN8092 is an Ethylene-Vinyl Acetate copolymer (EVA) which has a molecular structure that provides easy processing, adhesion, resilience, low hardness, good moisture, and gas barrier properties. It i.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | Injection-molding |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Melt Temperature | 225 - 250 °C | 437 - 482 °F | |
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Melt Temperature | 225 - 235 °C | 437 - 455 °F | |
NOVA Chemicals Sclair® 14B1 Butene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, heat resistance and barrier properties.Applications: Lamination, co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 225 °C | 437 °F | Optimum; Injection Molding |
DuPont Performance Polymers Hytrel® 4068FG TPC-ET
(Unverified Data**) Hytrel® 4068FG is a high performance thermoplastic polyester elastomer with food compliance specificity.Information provided by DuPont Performance Polymers |