Polymer Property : Melt Temperature = 518 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 270 - 320 °C
518 - 608 °F
PolyOne Edgetek® QT-20MN/000 natural HI Syndiotactic Polystyrene (SPS)
Information provided by PolyOne
Melt Temperature 270 °C
518 °F
DAM; Optimum
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
Zytel® 73G30T BK261 is a 30% glass fiber reinforced, toughened, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Melt Temperature 270 - 295 °C
518 - 563 °F
Injection Molding
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Melt Temperature 270 - 290 °C
518 - 554 °F
ISO 294
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Melt Temperature 270 - 290 °C
518 - 554 °F
ISO 294
Gromax BFG30-FU00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Melt Temperature 270 - 290 °C
518 - 554 °F
Recommended
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Melt Temperature 270 °C
518 °F
for test specimens; ISO 294
Lanxess Pocan® ECO T 3215 000000 PBT + PET, 15% Glass Fiber
PBT + PET, 15% glass fibers, injection molding, improved surface finish, contains 30% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
Melt Temperature 270 - 290 °C
518 - 554 °F
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn..
Melt Temperature 270 - 290 °C
518 - 554 °F
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Eu..
Melt Temperature 270 - 290 °C
518 - 554 °F
ISO 294
Gromax BFG30-FH00B1 Nylon 6 30% Glass Filled (Conditioned)
Information provided by Gromax Enterprises Corp.
Melt Temperature 270 - 287 °C
518 - 549 °F
ISO 294
Gromax BTG30-DN03N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
Melt Temperature 270 - 290 °C
518 - 554 °F
Lanxess Durethan® DP BKV 60 EF 000000 Nylon6, 60% Glass Fiber
PA 6, 60% glass fibers, injection molding, improved flowabilityInformation provided by LANXESS.
Melt Temperature 270 - 290 °C
518 - 554 °F
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica..
Melt Temperature 270 - 290 °C
518 - 554 °F
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Melt Temperature 270 - 295 °C
518 - 563 °F
Sax Polymers SAXAMID 126F4MW4 Nylon 6, 40% Glass Fiber and Mineral Reinforced
SAXAMID 126F4MW4 is a 40% glass fibers/ mineral reinforced polyamide 6 injection-molding-grade. It has dimensional stability and high strength.Information provided by SAX Polymers
Melt Temperature 270 - 290 °C
518 - 554 °F
A. Schulman SCHULAMID® 66 PTFE20 HS 20% PTFE Lubricated, Heat Stabilized Nylon 6/6
Information provided by A. Schulman.
Melt Temperature 270 - 300 °C
518 - 572 °F
Toyobo GLAMIDE® T-665C30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Melt Temperature 270 - 295 °C
518 - 563 °F
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned
Information provided by CP-Polymer-Technik GmbH & Co. KG
Melt Temperature 270 - 290 °C
518 - 554 °F
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF00ASXP PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXP is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as Staramide 66 G 50V S3)Information provided by Eurostar.
Melt Temperature 270 - 290 °C
518 - 554 °F
Eurostar Staramide RF00ASXS PA66, 50% Glass Filled, Injection Molded
Staramide RF00ASXA is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 270 - 285 °C
518 - 545 °F
Eurostar Starflam AFR450B PA66, 25% Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B is a Flame Retardant, 25% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Melt Temperature 270 - 290 °C
518 - 554 °F
Injection-molding/Extrusion
BASF Ultramid® B3EG6 30% Glass Filled PA6 (Dry)
Ultramid B3EG6 is a 30% glass fiber reinforced injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Melt Temperature 270 - 290 °C
518 - 554 °F
Injection-molding/Extrusion
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Dry)
Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability.
Melt Temperature 270 - 295 °C
518 - 563 °F
BASF Ultramid® HPN 9233G HS BK 102 33% Glass Filled PA6 (Dry)
Description: Ultramid HPN 9233G HS BK-102 is a heat stabilized, pigmented black, 33% glass reinforced PA6 injection molding grade resin in the High Productivity Nylon Series developed for improved c..
Melt Temperature 270 - 290 °C
518 - 554 °F
Injection molding
BASF Ultramid® S3WG7 Balance 35% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
Melt Temperature 270 °C
518 °F
DAM; Optimum; Injection Molding
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6  (Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
Melt Temperature 270 °C
518 °F
for shrinkage test
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET
Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, ..
Melt Temperature 270 - 290 °C
518 - 554 °F
Injection Molding/Extrusion
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
Melt Temperature 270 °C
518 °F
for shrinkage test, Optimal
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..