Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.70 mm |
>= 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-EN-FR3 Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.70 mm |
>= 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.70 mm |
>= 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.70 mm |
>= 120 sec @Thickness 0.0669 in |
UL 746 |
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
ALL |
Hexion Bakelite™ PF 31 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, standard molding compound for normal stress, UL listed molding compound 1.5 mm/V-1 (All), 3 mm/V-0 (All), standardized molding compound.Applicat.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
BK, BN |
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, .. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
BN, BK |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746 |
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance.Features: Bro.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
All colors; PLC 0 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.900 mm |
>= 120 sec @Thickness 0.0354 in |
BK; PLC 0 |
Eurostar Starflam RF0057E PA66, 25% Glass Filled, Injection Molded Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
PLC 0 |
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
PLC 0 |
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
All colors; PLC 0 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
BK; PLC 0 |
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.800 mm |
>= 120 sec @Thickness 0.0315 in |
PLC 0 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
PLC 0 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.750 mm |
>= 120 sec @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 3.00 mm |
>= 120 sec @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 0.750 mm |
>= 120 sec @Thickness 0.0295 in |
UL 746A |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746B |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
(BK) |
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,.. |
|||
Hot Wire Ignition, HWI | >= 120 sec @Thickness 1.50 mm |
>= 120 sec @Thickness 0.0591 in |
UL 746A |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |