Polymer Property : Electrical Resistivity = 0.0000250 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000250 ohm-cm
0.0000250 ohm-cm
Indium Corp. Indalloy® 205 In-Pb Solder Alloy
Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics..
Electrical Resistivity 0.0000250 ohm-cm
0.0000250 ohm-cm
Temperature Coefficient of 0.0013/K
Goodfellow Platinum 90/Iridium 10 Alloy
The alloy has been used in "non-standard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.Information provided ..