Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.0000250 ohm-cm | 0.0000250 ohm-cm | |
Indium Corp. Indalloy® 205 In-Pb Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Electrical Resistivity | 0.0000250 ohm-cm | 0.0000250 ohm-cm | Temperature Coefficient of 0.0013/K |
Goodfellow Platinum 90/Iridium 10 Alloy The alloy has been used in "non-standard" thermocouples, electrical contacts and for electrodes in medical research. The alloy is harder and mechanically stronger than Platinum.Information provided .. |