Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 6.00e+10 ohm-cm @Temperature 800 °C |
6.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Quartzel® Fused Quartz Textiles Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is ava.. |
|||
Electrical Resistivity | 6.00e+10 ohm-cm @Temperature 800 °C |
6.00e+10 ohm-cm @Temperature 1470 °F |
|
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Electrical Resistivity | 6.00e+10 ohm-cm | 6.00e+10 ohm-cm | |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |