Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+8 - 9.90e+10 ohm-cm
1.00e+8 - 9.90e+10 ohm-cm
Average value: 2.02e+10 ohm-cm Grade Count:6
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Electrical Resistivity 1.00 - 9.90e+10 ohm-cm
1.00 - 9.90e+10 ohm-cm
Average value: 2.22e+9 ohm-cm Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..