Polymer Property : Surface Resistance = 2.80e+14 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 2.80e+14 ohm
2.80e+14 ohm
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive
Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e..
Surface Resistance 2.80e+14 ohm
2.80e+14 ohm
Cond. A
Abatron AboCast/AboCure 8502-1 Epoxy
AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v..