Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 2.80e+14 ohm | 2.80e+14 ohm | |
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |
|||
Surface Resistance | 2.80e+14 ohm | 2.80e+14 ohm | Cond. A |
Abatron AboCast/AboCure 8502-1 Epoxy AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v.. |