Electrical Properties | Metric | English | Comments |
---|---|---|---|
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val.. |
|||
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plenco 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 5000 is the replacement material for the former Union Carbide BMM-5000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding performance and preheating cha.. |
|||
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics.. |
|||
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Comparative Tracking Index | 140 V | 140 V | per 50 drops; ASTM D3638 |
Gharda Chemicals G-PAEK™ 1230GF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% glass fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, standard flow, Beige .. |
|||
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plaslok 5000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 5000 is the replacement material for .. |
|||
Comparative Tracking Index | 140 V | 140 V | UL 746 |
Plaslok 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 7000 is the replacement material for .. |