Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **)

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7000 Black General Purpose Woodflour Filled Phenolic Molding Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plaslok 7000 is the replacement material for the former Union Carbide BMM-7000. It is a two-stage, woodflour-filled phenolic molding compound having versatile molding and preheating characteristics, fast cure, low specific gravity and excellent molded surface finish.Data provided by Plaslok Corporation.Plaslok Corporation was purchased by Plastics Engineering Company in March 2000. The Plaslok name is no longer used on any products.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Water Absorption 0.45 %
0.45 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Compression; ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Flexural Yield Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Compressive Yield Strength 234 MPa
33900 psi
ASTM D695
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
331 °F
ASTM D648
UL RTI, Electrical 150 °C

@Thickness 1.47 mm
302 °F

@Thickness 0.0579 in
UL RTI, Mechanical with Impact 150 °C

@Thickness 1.47 mm
302 °F

@Thickness 0.0579 in
UL RTI, Mechanical without Impact 150 °C

@Thickness 1.47 mm
302 °F

@Thickness 0.0579 in
Flammability, UL94 HB

@Thickness 3.05 mm
HB

@Thickness 0.120 in
HB

@Thickness 3.05 mm
HB

@Thickness 0.120 in
Electrical Properties Metric English Comments
Electrical Resistivity 3.00e+12 ohm-cm
3.00e+12 ohm-cm
ASTM D257
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
ASTM D150
6.0

@Frequency 60 Hz
6.0

@Frequency 60 Hz
ASTM D150
Dielectric Strength 13.8 kV/mm
351 kV/in
ASTM D149
Dissipation Factor 0.040

@Frequency 1e+6 Hz
0.040

@Frequency 1e+6 Hz
ASTM D150
0.070

@Frequency 60 Hz
0.070

@Frequency 60 Hz
ASTM D150
Comparative Tracking Index 140 V
140 V
UL 746