Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 260 sec | 260 sec | |
Mykroy/Mycalex MM 500 Machining Grade Glass-bonded Mica Composite Synthetic mica filler. Does not burn. Better radiation resistance (3 x 10^10 Rads-Cobalt) than grade 400.This ceramoplastic material is a versatile and efficient insulating material designed to me.. |
|||
Arc Resistance | 260 sec | 260 sec | |
Pyrotek Hirolex HG Electrical Insulating Material Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.Information provided by Pyrotek. |
|||
Arc Resistance | 260 sec | 260 sec | |
Pyrotek NAD-250 Structural Insulation Board NAD-250 is a general purpose cement board. It is suitable for low-voltage electrical insulation in dry conditions.ApplicationsOven shelves Platen insulators Coil boxes Foundry core plates Heat guar.. |
|||
Arc Resistance | 260 sec | 260 sec | ASTM D495 |
BNZ Materials Transite HT Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |