Polymer Property : Shielding Effectiveness = 30 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
Parker Chomerics COMBO® and COMBO® Strip Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel ..
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
Parker Chomerics Frame Gasketing Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInf..
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
Parker Chomerics MESH STRIP™ (all metal) Wire Mesh EMI Gasket Selection Guide
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Strips, Gaskets Made by Joining Strips.Standard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by C..
Shielding Effectiveness 25 - 30 dB

@Frequency 14000 Hz
25 - 30 dB

@Frequency 14000 Hz
Parker Chomerics SHIELDMESH™ Wire Mesh EMI Gasket Selection Guide
Construction: Formed or Compressed Knitted Wire MeshAvailable Forms: Jointless Rings or Rectangular GasketsStandard Metals Available in EMI Portion: Monel Ferrex, Aluminum.Information provided by Ch..
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
Parker Chomerics COMBO® Gaskets Wire Mesh EMI Gasket Selection Guide
Construction: Formed Knitted Wire Strips in Parallel with Elastomer Strips; or Die-Cut GasketsAvailable Forms: Die-Cut Elastomer with Joined EMI Strips.Standard Metals Available in EMI Portion: Mone..