Construction: Formed Knitted Wire Strips Clamped in Aluminum ExtrusionsAvailable Forms: Strips, Fab. Lengths, Frames with Joined EMI Strips..Standard Metals Available in EMI Portion: Monel FerrexInformation provided by Chomerics
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 66.0 °C
151 °F
Neoprene Version
204 °C
399 °F
Silicone Version
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Silicone Version
-34.0 °C
-29.2 °F
Neoprene Version
Electrical Properties Metric English Comments
Shielding Effectiveness 20 - 30 dB

@Frequency 14000 Hz
20 - 30 dB

@Frequency 14000 Hz
>= 93 dB

@Frequency 1.00e+9 Hz
>= 93 dB

@Frequency 1.00e+9 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
>= 102 dB

@Frequency 1.80e+7 Hz
Descriptive Properties Value Comments
Maximum Joint Unevenness, % of Gasket Height 0.25
Class B- Open-Close in Same Position
0.25
Class C- Completely Interchangeable
0.3
Class A- Permanently Closed