Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 90 dB @Frequency 5.00e+8 Hz |
90 dB @Frequency 5.00e+8 Hz |
E-Field; Mil-G-83528/MIL std 285 |
P & P Technology Nickel Graphite Loaded EPDM Molding grade conductive EPDM elastomer loaded with nickel graphite filler. The material is dark grey in color and is specially compounded to give high EMC performance and excellent IP sealing.Infor.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 1.00e+10 Hz |
>= 90 dB @Frequency 1.00e+10 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 1.00e+10 Hz |
>= 90 dB @Frequency 1.00e+10 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 2.00e+9 Hz |
>= 90 dB @Frequency 2.00e+9 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB @Frequency 1.00e+10 Hz |
>= 90 dB @Frequency 1.00e+10 Hz |
Plane Wave; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | >= 90 dB @Frequency 1.00e+8 Hz |
>= 90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 5.00e+8 Hz |
>= 90 dB @Frequency 5.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal.. |
|||
Shielding Effectiveness | 90 dB @Frequency 2.00e+8 Hz |
90 dB @Frequency 2.00e+8 Hz |
26 in. x 26 in. test panel; TP08 Modified |
Parker Chomerics CHO-SHIELD® 2056 Conductive Coating CHO-SHIELD® 2054 silver-plated-copper filled commercial-grade coating proved high levels of EMI shielding effectiveness, abrasion resistance and excellent adhesion on a variety of materials used fo.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics ECOPLATE™ 5030 Description: ECOPLATE™ 5030 is a pure metal wire with a metallurgical composition free of defects or contaminates. When applied with the automated ECOPLATE process, it conforms to the substrate muc.. |
|||
Shielding Effectiveness | 90 dB @Frequency 5.00e+8 Hz |
90 dB @Frequency 5.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics ECOPLATE™ 5030 Description: ECOPLATE™ 5030 is a pure metal wire with a metallurgical composition free of defects or contaminates. When applied with the automated ECOPLATE process, it conforms to the substrate muc.. |
|||
Shielding Effectiveness | 90 dB @Frequency 2.00e+9 Hz |
90 dB @Frequency 2.00e+9 Hz |
CHO-TM-TP08 |
Parker Chomerics ECOPLATE™ 5030 Description: ECOPLATE™ 5030 is a pure metal wire with a metallurgical composition free of defects or contaminates. When applied with the automated ECOPLATE process, it conforms to the substrate muc.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+10 Hz |
90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 1.00e+10 Hz |
>= 90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer Description: CONSIL-E is a continuously extruded silicone elastomer filled with silver-plated inert particles. It is a medium hardness material providing high electrical conductivity and moisture se.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+10 Hz |
90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+10 Hz |
90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+10 Hz |
90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+7 Hz |
90 dB @Frequency 1.00e+7 Hz |
E-Field |
Parker Chomerics Tecknit ECTC™ Windows Electrically Conductive Transparent Coating Description: ECTC WINDOWS are custom designed optical display panels produced by depositing a very thin electrically conductive transparent coating directly onto the surface of various optical subst.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+9 Hz |
90 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+10 Hz |
90 dB @Frequency 1.00e+10 Hz |
Plane Wave |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 2.00e+9 Hz |
>= 90 dB @Frequency 2.00e+9 Hz |
Plane Wave; CHO-TM-TP08 |
Parker Chomerics CHO-SEAL 1310 Conductive Elastomer Moderate performance in non-corrosive environments, no corrosion or fluid resistance; material of choice for small, delicate injection-molded parts or large dimension extrusionsMolded onlyRoHS Compl.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 5.00e+8 Hz |
>= 90 dB @Frequency 5.00e+8 Hz |
E-Field; Method 2, MIL-DTL-83528 Para. 4.6.12 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Shielding Effectiveness | 90 dB @Frequency 4.00e+9 Hz |
90 dB @Frequency 4.00e+9 Hz |
|
Parker Chomerics SOFT-SHIELD® 1000 Low Closure Force, Foam Core EMI Gasket Description: Easy-to-install SOFT-SHIELD® 1000 Series gaskets are specially designed for shielding commercial electronic enclosures with tight space constraints or low closure force requirements. T.. |
|||
Shielding Effectiveness | 90 dB @Frequency 4.00e+9 Hz |
90 dB @Frequency 4.00e+9 Hz |
|
Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket Description: SOFT-SHIELD® 2000 Series gaskets consist of silver-plated nylon yarn knitted as the outer layer over a highly compressible, thermoplastic EPDM foam core. Through a special treatment pr.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |
|||
Shielding Effectiveness | 90 - 100 dB @Frequency 2.00e+9 - 3.00e+9 Hz |
90 - 100 dB @Frequency 2.00e+9 - 3.00e+9 Hz |
|
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding Description: Master Bond MB600S is a silver containing aqueous based sodium silicate system used as a coating in situations where EMI shielding effectiveness is paramount. Electromagnetic interferen.. |
|||
Shielding Effectiveness | >= 90 dB @Frequency 4.00e+10 Hz |
>= 90 dB @Frequency 4.00e+10 Hz |
Plane Wave; MIL-DLT-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Shielding Effectiveness | 90 dB @Frequency 1.00e+8 Hz |
90 dB @Frequency 1.00e+8 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu.. |