Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® FXS610SK ABS (Europe-Africa-Middle East) CYCOLAC FXS610SK is a multi purpose ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC FXS610SK is suitable for those applications that require sparkle c.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® G360 ABS (Europe-Africa-Middle East) CYCOLAC G360 is a high flow, high impact, medium to high heat resistant injection moulding ABS grade. It is recommended for large or complex parts in the automotive or electrical power tool segments.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S701SU ABS (Europe-Africa-Middle East) CYCOLAC S701SU is an ABS with improved UV resistance, providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an exce.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S702S ABS (Europe-Africa-Middle East) CYCOLAC S702S is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries. Cycolac S702S is anti-dust equiped.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S705 ABS (Europe-Africa-Middle East) CYCOLAC S705 is a new generation ABS plating grade, offering semi high heat with a good property balance for impact and flow. CYCOLAC S705 demonstrates excellent electroplatability and a good therma.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® CRT3370 ABS (Europe-Africa-Middle East) CYCOLAC CRT3370 is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow char.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 2200N PEI 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2210F PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl LS175 PPE+HIPS Noryl* LS175 modified polyphenylene ether resin is an unfilled grade suitable for both extrusion and injection molding conversion routes. It uses non-chlorinated, non-brominated FR additives to del.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm, Temperature 23.0 °C |
660 kV/in @Thickness 0.0787 in, Temperature 73.4 °F |
DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This .. |