Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® G366 ABS (Europe-Africa-Middle East) CYCOLAC G366 is a "new technology" grade of ABS exhibiting outstanding property balance, a good flow, medium impact, medium to high heat resistant and an excellent stability during injection mouldin.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® S708C ABS (Europe-Africa-Middle East) Cycolac* S708C is an improved scratch resistant ABS product with high stiffness and heat, used for applications in appliances, telecom, business machines and TV industries.This data was supplied by .. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® X37 ABS (Europe-Africa-Middle East) CYCOLAC X37 is the highest heat material available in the CYCOLAC range of materials and is widely recognized within the automotive industry as being the industry standard for high heat ABS. It comb.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East) Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V01550 PPE+HIPS (Europe-Africa-Middle East) NORYL V01550 is a 15 % short glass fibre reinforced, flame retardant material with a HDT/A of 130C according ISO 75. NORYL V01550 is V0 at 0.75 mm according UL94 and is halogen free according VDE/DI.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2210 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics ULTEM CRS5201 PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. Resin is RoHS compliant. UL94 V0 and 5VA li.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 0.800 mm |
660 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 0.800 mm |
660 kV/in @Thickness 0.0315 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL PX2245 PPE+HIPS (Europe-Africa-Middle East) NORYL PX2245 is a halogen free (according to VDE/DIN 472 part815) flame retardant material. The material fulfills the IEC 65 part 20.2 requirement at 1.6 mm thickness. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-521 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm |
660 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 2.00 mm, Temperature 23.0 °C |
660 kV/in @Thickness 0.0787 in, Temperature 73.4 °F |
DAM; IEC 60243-1 |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Dielectric Strength | 26.0 kV/mm @Thickness 1.60 mm |
660 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Cycolac® CRT3370F ABS (Europe-Africa-Middle East) CYCOLAC CRT3370F is a 17% glass reinforced injection moulding grade of ABS. It exhibits high rigidity and excellent dimensional stability combined with medium/high heat performance and good flow cha.. |