Polymer Property : Dielectric Strength = 500 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm

@Thickness 3.17 mm
500 kV/in

@Thickness 0.125 in
in oil; ASTM D149
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant
Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
D-48/50
Industrial Laminates/Norplex NP180 Synthetic Fabric  (discontinued **)
Description: aramid fabric material with a high performance epoxy resin matrix. Excellent electrical and mechanical properties at elevated temperatures and in adverse environments.Thickness Tested: ..
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP101 Synthetic Fabric
Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp..
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP320E Cotton Fabric
Description: Similar to NP320 with improved moisture resistance. Suitable for electrical applications in moderate humidity conditions.Thickness Tested: 0.062", 0.125", and 0.500”
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond D-48/50; ASTM D229 S.T.
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP660 Paper Base Laminate
Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500"
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Dielectric Strength 19.7 kV/mm

@Thickness 1.57 mm
500 kV/in

@Thickness 0.0620 in
Cond A; ASTM D229 S.T.
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
Dielectric Strength 19.7 kV/mm

@Thickness 1.02 mm
500 kV/in

@Thickness 0.0400 in
ASTM-D149
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film
Applications: thin film substrates
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7620-T Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7660-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7690-T Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-Tand 7690-T Series, contain one-piece, non-skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 for indo..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7640-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7650-S Cold Shrink Silicone Rubber Termination Kits QT-III
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7640-S, 7650-S and 7660-S Series, contains one-piece, skirted, silicone rubber termination, qualified as IEEE Standard 48 Class 1 fo..
Dielectric Strength 19.7 kV/mm

@Thickness 1.91 mm
500 kV/in

@Thickness 0.0750 in
Silicone Rubber Insulator; ASTM D149
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Dielectric Strength 19.7 kV/mm

@Thickness 3.20 mm
500 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer..