Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm, Temperature 23.0 °C |
584 kV/in @Thickness 0.0630 in, Temperature 73.4 °F |
Short Time; ASTM D149 |
DuPont Performance Polymers Crastin® ST820 BK503 PBT
(Unverified Data**) Crastin® ST820 BK503 is an unreinforced, Super Tough, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
Conditioned; ASTM D149 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 0.800 mm |
584 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 0.800 mm |
584 kV/in @Thickness 0.0315 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 3.20 mm |
584 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 745 PBT (Europe-Africa-Middle East) VALOX 745 is 30% mineral filled PBT injection moulding resin with improved toughness and low warpage. Applications: telephone ringer frames, card racks. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 771 PBT (Europe-Africa-Middle East) VALOX 771 is a 15% glass and 20% mineral filled, flame retarded injection moulding PBT resin. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® DR48V PBT (Europe-Africa-Middle East) VALOX DR48V is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 1.60 mm |
584 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-400G15 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-602G30 MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Practical Use (Water Absorption 1.7%); ASTM-D149 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
Absolute Drying; ASTM-D149 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm, Temperature 90.0 °C |
584 kV/in @Thickness 0.0787 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm, Temperature 90.0 °C |
584 kV/in @Thickness 0.0787 in, Temperature 194 °F |
IEC 60243-1 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
Dielectric Strength | 23.0 kV/mm @Thickness 2.00 mm |
584 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |