Electrical Properties | Metric | English | Comments |
---|---|---|---|
Insulation Resistance | 5.00e+9 ohm @Diameter 8.00 - 10.0 mm |
5.00e+9 ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments.. |
|||
Insulation Resistance | 5.00e+9 ohm @Diameter 8.00 - 10.0 mm |
5.00e+9 ohm @Diameter 0.315 - 0.394 in |
24hr/50°C+24h in water at 23°C; IEC; IEC/EN 61212-2 6.2 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac.. |
|||
Insulation Resistance | >= 5.00e+9 ohm | >= 5.00e+9 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GM 202 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Insulation Resistance | >= 5.00e+9 ohm | >= 5.00e+9 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GM 201 Glass Mat Reinforced Epoxy Resin - Sheet Used in mechanical and electrical applications. Extremely high mechanical strength at moderate temperature. Very good electrical properties under high humidity.Information provided by Hippe. |
|||
Insulation Resistance | >= 5.00e+9 ohm | >= 5.00e+9 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
Insulation Resistance | >= 5.00e+9 ohm | >= 5.00e+9 ohm | After immersion in water; IEC 1212-2 6.3 |
Hippe EP GM 204 Glass Mat Reinforced Epoxy Resin - Sheet |