Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Breakdown | >= 20000 V @Temperature 90.0 - 90.0 °C |
>= 20000 V @Temperature 194 - 194 °F |
Average value: 23300 V Grade Count:6 |
Overview of materials for Phenolic, Novolac, Cellulose Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Cellulose Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 - 90.0 °C |
>= 20000 V @Temperature 194 - 194 °F |
Average value: 30000 V Grade Count:2 |
Overview of materials for Phenolic/Glass Fiber SMC This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Glass Fiber SMC". Each property range of values reported is minimum and maximum values of appro.. |
|||
Dielectric Breakdown | 20000 V @Thickness 1.57 mm |
20000 V @Thickness 0.0620 in |
Cond A; ASTM D229 S/S |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Dielectric Breakdown | 20000 V | 20000 V | 1hr 94C; ASTM D149 |
Plenco 1500 Polyester, Granular, Transfer Molded PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon.. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe EP CP 201 Cellulose Paper Reinforced Epoxy Resin - Sheet Used in electronic applications. Good stability of electrical properties under high humidity. Flame retardant.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CC 204 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CP 203 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CP 205 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions. Flame retardant.Information provided .. |
|||
Dielectric Breakdown | 20000 V | 20000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® EL21 Polyester Film, 1400 Gauge Mylar® EL21 polyester films are flexible strong and durable films with an unusual balance of properties, making them suitable for a variety of industrial applications. The excellent dielectric stre.. |
|||
Dielectric Breakdown | 20000 V | 20000 V | 1/4" electrode 500 V/sec 25°C in air; ASTM D149 |
DuPont Teijin Films Mylar® MO21 Polyester Film, 1400 Gauge Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moistur.. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe. |
|||
Dielectric Breakdown | >= 20000 V | >= 20000 V | ASTM D1000 |
3M Scotchrap™ 51 Tape 3M™ Scotchrap™ Tapes 50 and 51 are tough, polyvinyl chloride based tapes with special high tack adhesives formulated to resist corrosion of metal piping systems above and below ground, fittings an.. |
|||
Dielectric Breakdown | >= 20000 V @Temperature 90.0 °C |
>= 20000 V @Temperature 194 °F |
In oil, parallel to laminations; IEC 1212-2 6.2 |
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe. |