Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | PLC code 1; UL 746A |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746 |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycolac® EX58F ABS (Asia Pacific) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | Average value: 15.8 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 50.0 mm/min | 0.394 - 1.97 in/min | Average value: 32.7 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS High impact and ductility at 73F (23C) and -20F (-29C). |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 50.0 mm/min | 0.394 - 1.97 in/min | Average value: 32.7 mm/min Grade Count:4 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 150 mm/min | 0.394 - 5.91 in/min | Average value: 38.6 mm/min Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 150 mm/min | 0.394 - 5.91 in/min | Average value: 102 mm/min Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 3.00 mm |
0.394 - 1.00 in/min @Thickness 0.118 in |
ALL |
Hexion Bakelite™ PF 2400 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof, UL Listed
(disc Phenolic molding compound, inorganically/organically filled, average heat resistance, increased dimensional stability, dish washer proof, UL listed molding compound 1.5 mm/V-0 (ALL).Application area.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 20HRI GPPS Heat resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, S.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical 65IH HIPS High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: Food Container, Merchandise, Artificial Woods, Refrigerator Vegetable Box, PSP, Sheet, Film, etc.CAS: 9003-53-6-5In.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUMID GP3150A(W) PA6+MF15%, General Purpose Feature: Injection Molding, PA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 25SPI GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min | <= 0.394 in/min | UL Rating PLC 0 (0-10 mm/min) |
LG Chemical 92HR SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include automobile battery cases, water meter case.. |
|||
High Voltage Arc-Tracking Rate, HVTR | <= 10.0 mm/min @Thickness 3.18 mm |
<= 0.394 in/min @Thickness 0.125 in |
UL Rating PLC 0 (<10 mm/min.) |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000LG PC, Transparent Description: Injection Molding, PC, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsInformation provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Valox® DR51 PBT (Asia Pacific) 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL 746A |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min @Thickness 3.00 mm |
0.394 - 1.00 in/min @Thickness 0.118 in |
UL Rating PLC 1 (10-25.4 mm/min.) |
Covestro Makrolon® 3258 Polycarbonate, General Purpose, Mold Release, Biocompatibility It is the responsibility of the medical device, biological product, or pharmaceutical manufacturer (Manufacturer) to determine the suitability of all component parts and raw materials, including the.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |
LG Chemical 402 AF Flame Retardant HIPS NON-DECA, Flame retardant, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include t.. |