Polymer Property : Dielectric Strength = 10.4 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 10.4 kV/mm

@Thickness 3.20 mm
264 kV/in

@Thickness 0.126 in
Short-Time 500 V/sec
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Dielectric Strength 10.4 kV/mm
264 kV/in
Short Time; ASTM D149
Plenco 2424 Phenolic, Granular, Injection Molded  (discontinued **)
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical ..
Dielectric Strength 10.4 kV/mm
264 kV/in
Step by Step; ASTM D149
Plenco 00714 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Dielectric Strength 10.4 kV/mm
264 kV/in
Short Time; Dry; ASTM D149
Resinoid 2018 Phenolic Molding, Fabric Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance