Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.8 kV/mm | 275 kV/in | Short Term; ASTM D149 |
Quadrant EPP Fluorosint® 500 PTFE, synthetic mica-filled PTFE, compression molded (ASTM Product Data Sheet) |
|||
Dielectric Strength | 10.8 kV/mm | 275 kV/in | Short Term |
Saint-Gobain Rulon® E Grade Bearing/Seal PTFE
(discontinued **) Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of friction, and .. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Short Time; ASTM D149 |
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group. |
|||
Dielectric Strength | 10.8 - 14.7 kV/mm | 274 - 373 kV/in | Average value: 12.5 kV/mm Grade Count:10 |
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum .. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade Durez 152 Phenolic is a two-stage, heat resistant/electrical molding material. It exhibits superior dimensional stability, good strength retention at elevated temperature and good molded appearance.. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 156 Phenolic, Compression Grade Durez 156 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits excellent dimensional stability, high heat resistance, good molded appearance, and UL.. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |
|||
Dielectric Strength | 10.8 kV/mm | 274 kV/in | Step by step; ASTM D149 |
Sumitomo Bakelite Durez® 31906 Phenolic, Compression Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Dielectric Strength | 10.8 - 12.8 kV/mm | 275 - 325 kV/in | short time |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Dielectric Strength | 10.8 - 12.8 kV/mm | 275 - 325 kV/in | short time |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |