Electrical Properties Metric English Comments
Dielectric Strength >= 4.00 kV/mm

@Thickness 1.00 mm
>= 102 kV/in

@Thickness 0.0394 in
in oil; ASTM D149
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific)
Thermally conductive electrically insulative mineral filled PPS FR compound.
Dielectric Strength 4.00 kV/mm
102 kV/in
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal
Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam..
Dielectric Strength 4.00 kV/mm
102 kV/in
AC 60 Hz
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 4.00 kV/mm
102 kV/in
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 4.00 kV/mm
102 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 4.00 kV/mm
102 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 4.00 kV/mm
102 kV/in
60°C for 500 hrs
Fujipoly Industries Sarcon® 30H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Strength 4.00 kV/mm
102 kV/in
1 MHz
Momentive Performance Materials Type 214 Fused Quartz Tubing
Used for clear fused quartz lamp tubing. GE 214 is a high purity, high transmittance, high temperature material with a low hydroxyl (OH-) content. It is suitable for a broad range of mercury, halo..
Dielectric Strength 4.00 kV/mm
102 kV/in
IEC 60243
Solvay TECHNYL® A 246M PA66, Conditioned
Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN..
Dielectric Strength 4.00 kV/mm

@Thickness 0.100 mm
102 kV/in

@Thickness 0.00394 in
ASTM D149
Solvay Specialty Polymers Ajediumâ„¢ Films PPS Polyphenylene Sulfide (PPS)
Polyphenylene sulfide, PPS, is a thermoplastic film that has excellent chemical resistance and good electrical and physical properties.Features: Flame Retardant; Good Chemical Resistance; Good Elect..
Dielectric Strength 4.00 kV/mm
102 kV/in
ASTM D149
Tipco Tipcolite® TG 613 Phenolic Compound, Mineral & Wood Flour, Soft Flow & Good Surface Finish
Soft Flow Phenolic Compound, Reinforced with Mineral & Wood FlourApplications: General PurposeProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India...
Dielectric Strength >= 4.00 kV/mm

@Temperature 90.0 °C
>= 102 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATM 123 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownMedium flow..
Dielectric Strength 4.00 - 5.50 kV/mm

@Temperature 90.0 °C
102 - 140 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATO 176 Phenolic Molding Organic and inorganic Filler, Compression Molded
Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackMedium flow App..
Dielectric Strength 4.00 - 5.00 kV/mm

@Temperature 90.0 °C
102 - 127 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni..