Polymer Property : Dielectric Strength = 16.3 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in air; ASTM D149
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific)
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only.
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Lexan® 193 PC
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. UV-stabilized. Opaques only.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in air; ASTM D 149
SABIC Innovative Plastics Lexan® 194 PC
Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region.
Dielectric Strength 16.3 kV/mm

@Thickness 0.800 mm
414 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Asia Pacific)
Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce..
Dielectric Strength 16.3 kV/mm

@Thickness 0.800 mm
414 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Dielectric Strength 16.3 kV/mm

@Thickness 0.800 mm
414 kV/in

@Thickness 0.0315 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Dielectric Strength 16.3 kV/mm

@Thickness 0.800 mm
414 kV/in

@Thickness 0.0315 in
in oil; ASTM D 149
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics Lexan® LGK5030 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Dielectric Strength 16.3 kV/mm
414 kV/in
Short Time; ASTM D149
Plenco 50030 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..
Dielectric Strength 16.3 kV/mm
415 kV/in
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive
1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t..
Dielectric Strength 16.3 kV/mm
415 kV/in
Taiwan PU Corporation TPUCO Polyurethane Sealing Resin
PU sealing resin is a waterproof, insulated protective film made of quality PU resin. It is used in the prevention of humidity, germs, collision, corrosion, parts loosening, and rusting, and as ins..
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC
LNP* Thermocomp* Lexan_LGN5030 compound is a glass reinforced. Flame retardant.
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Asia Pacific)
Glass reinforced. Flame retardant.
Dielectric Strength 16.3 kV/mm

@Thickness 3.20 mm
414 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics LNP THERMOCOMP Lexan_LGK5030 PC (Europe-Africa-Middle East)
LNP* Thermocomp* Lexan_LGK5020 compound is a glass reinforced, flame retardant material.
Dielectric Strength 16.3 kV/mm
414 kV/in
Short Time; ASTM D149
Plenco 3356 Phenolic, Granular, Compression Molded
PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i..
Dielectric Strength 16.3 kV/mm
414 kV/in
Short Time; ASTM D149
Plenco 6015 Phenolic, Briquette, Transfer Molded
PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf..
Dielectric Strength 16.3 kV/mm
415 kV/in
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound
TRA-BOND 2116 is a thixotropic, low vapor pressure epoxy system that passes the NASA Outgassing Specification. It is recommended for critical electronic, aerospace, and industrial applications where..
Dielectric Strength 16.3 kV/mm
414 kV/in
Eastman Eastar DN004 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Dielectric Strength 16.3 kV/mm
415 kV/in
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT
Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning
Dielectric Strength 16.3 kV/mm
414 kV/in
ASTM D149
Arlon 55629R028 0.0285" (0.724 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglassThis data repre..
Dielectric Strength 16.3 kV/mm
415 kV/in
ASTM D149
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use..